Типични характеристики
Метод
Gazpromneft Reductor CLP 68
Kinematic Viscosity
- at 40 °С, mm²/s
ASTM D 445
68
Flash Point (COC), °С
ASTM D 92
238
Pour Point, °С
ГОСТ 20287
- 20
Total Acid Number, mg KOH/g
0.7
Density
- at 20 °С, g/cm³
ASTM D 4052
0.883
Tribological characteristics, Four-Ball Method
- Load-wear index, N
- Wear Scar Diameter, mm
ГОСТ 9490
ГОСТ 9490
454
0.25
SAE viscosity class
ASTM D 2270
94
Corrosion of the copper
- 3 hours at 100 °C
ASTM D 130
1в